InspectMesh
Tools

Planning & calibration

3D Printer Fit Checker3D PrintersCompare 3D Printers3D Print Cost Calculator3D Printing Price CalculatorFilament Length CalculatorFlow Rate CalculatorTolerance & ClearanceShrinkage CalculatorOrientation PlannerBed Layout Planner

After slicing

G-code Viewer & Preflight
View all 3D tools
STL toolsSTL ViewerSTL Quality CheckerSTL Print Preflight CheckerSTL Repair ToolSTL Watertight CheckerSTL Manifold CheckerSTL Dimensions CheckerSTL Scale ToolSTL Wall Thickness CheckerSTL Overhang CheckerSTL SplitterSTL Volume CalculatorSTL Triangle CounterSTL File Size ReducerSTL to 3MF Converter
3MF tools3MF Viewer3MF Quality Checker3MF Print Preflight Checker3MF Repair Tool3MF Watertight Checker3MF Manifold Checker3MF Dimensions Checker3MF Wall Thickness Checker3MF Overhang Checker3MF Volume Calculator3MF Triangle Counter3MF to STL Converter
MaterialsGuidesExamplesContact
Home›Compare 3D Printing Materials›PA / Nylon vs Polycarbonate / PC

PA / Nylon vs Polycarbonate / PC: Which Filament Should You Use?

Nylon prioritises tough, wear-capable parts while PC raises heat resistance and printer demands.

Choose PA / Nylon when

  • You need toughness and can control moisture.

Choose Polycarbonate / PC when

  • High heat resistance is the deciding factor.

Requirements that decide this pair

RequirementPA / NylonPolycarbonate / PC
Service requirementInvestigate a grade when wear and toughness motivate the choice.Investigate a grade when loaded thermal service is the deciding requirement.
Dimensional evidenceDefine moisture conditioning before accepting measured fit.Define the blend, thermal process and cooled measurement state.
Available printerVerify drying, feed path and any abrasive reinforcement requirements.Verify the exact documented nozzle, bed and enclosure environment; hotend temperature alone is insufficient.

An engineering cover needs a grade-level qualification

A hypothetical 90 mm protective cover may require toughness, heat stability and accurate mounts. Nylon and PC are candidate families; compare exact datasheets at the operating temperature, moisture state and load. Print a dimensional coupon and final mounting geometry before choosing. Neither a family label nor a coupon certifies the assembled cover.

Hypothetical application, not an InspectMesh physical material test.

When the initial choice changes

A moisture-sensitive fit may change the nylon shortlist. A printer unable to hold the documented PC environment can remove PC from consideration even if its datasheet looks attractive. Blends and reinforced grades can reverse broad comparisons.

Evidence that would change this choice

Conditional choice: Choose between documented exact formulations and available hardware, rather than two engineering-family labels.

The examples are unfilled PA11 and PC Blend. Their printed specimens use different printers, thermal settings and slicers; mechanical conditioning is not specified. Read their separate values without a numerical winner.

Next evidence to collect: For the 90 mm engineering cover, keep moisture-conditioned mounting fit, thermal method/load and print capability as three decisions. Verify PA11 chamber capability and PC Blend surface/profile requirements. Its 93 °C at 1.80 MPa and 113 °C at 0.45 MPa are separate historical tests; unmatched PA11/PC data remain separate.

Interpret the two PC Blend test loads

Family context explains the trade-off above. The named examples below retain their own formulation and test scope.

Published product examples, separate from the family view

These are identified formulations chosen to show how to read evidence. Selecting a family does not select a brand for your part. HDT rows are grouped by reported test load, never by the highest temperature. An absent matching-load result remains unavailable; matching a load alone does not establish matching specimen or conditioning.

Prusament PA11 evidence · Prusament PC Blend evidence

Compare reported properties and conditions, without an overall winner
Property Prusament PA11 Prusament PC Blend Comparison scope
Density

1.02 g/cm³

Prusa Polymers, v1.0
Source conditions

Method: ISO 1183; load: not specified; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-10-29.

1.22 g/cm³

Prusa Polymers, v1.1
Source conditions

Method: Prusa Polymers; load: not specified; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-11-03.

Separate published values

Different or unspecified method, specimen, conditioning, test temperature. Read each source separately; these values do not establish which material performs better in your part.

Heat deflection temperature (1.80 MPa) Not found in this example; not zero.

93 °C

Prusa Polymers, v1.1
Source conditions

Method: ISO 75; load: 1.80 MPa; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-11-03.

Unavailable

A numeric result is not published for one or both selected examples. Missing is not zero.

Heat deflection temperature (0.45 MPa) Not found in this example; not zero.

113 °C

Prusa Polymers, v1.1
Source conditions

Method: ISO 75; load: 0.45 MPa; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-11-03.

Unavailable

A numeric result is not published for one or both selected examples. Missing is not zero.

Tensile modulus

1.2 ± 0 GPa

Prusa Polymers, v1.0
Source conditions

Method: ISO 527-1; load: not specified; specimen: CORE One+ firmware 6.4.0; 0.4 mm High-Flow CHT; PrusaSlicer 2.9.6; 0.20 mm layers; 100% rectilinear; 2 perimeters; no top/bottom; 275 °C nozzle; 100 °C bed; 55 °C chamber; orientation: Horizontal; conditioning: not specified; test temperature: not specified.

p. 2, printed-specimen table; p. 3, footnote setup. Checked 2026-10-29.

1.9 ± 0.1 GPa

Prusa Polymers, v1.1
Source conditions

Method: ISO 527-1; load: not specified; specimen: MK3S; PrusaSlicer 2.1.1; 0.20 mm FAST; 100% rectilinear infill; 2 perimeters; no top/bottom; 275 °C nozzle; 115 °C bed; orientation: Horizontal; conditioning: not specified; test temperature: not specified.

p. 2, printed-specimen table; p. 3, footnote setup. Checked 2026-11-03.

Separate published values

Different or unspecified specimen, conditioning, test temperature. Read each source separately; these values do not establish which material performs better in your part.

HDT is a loaded deflection test, not a continuous service limit. Modulus measures stiffness; it is not impact strength. Shore A and D remain different scales.

Open this pair in the comparison tool

Prepare the exact formulation

Both need product-specific thermal, surface and drying preparation. Verify printer material documentation and remeasure cooled/conditioned dimensions; do not infer support from a 300 C hotend alone.

Use the spool maker's settings and datasheet; a family-wide nozzle range is not a qualified profile.

Sources for this decision

  • Prusa Research: PA-NYLON material guidance (checked 2026-10-09)
  • Prusa Research: PC material guidance (checked 2026-10-09)

Sources describe the material families and printing preparation. Application dimensions and qualification steps above are illustrative design decisions.

PA / Nylon guide · Polycarbonate / PC guide · Use the selector

Reviewed 2026-11-03.

Get occasional updates on new tools and practical 3D-print guides.

Verification (required)

Enter your email to start verification.

Simple, browser-friendly tools for better 3D prints.

ExamplesPrivacyCookiesContact