InspectMesh
Tools

Planning & calibration

3D Printer Fit Checker3D PrintersCompare 3D Printers3D Print Cost Calculator3D Printing Price CalculatorFilament Length CalculatorFlow Rate CalculatorTolerance & ClearanceShrinkage CalculatorOrientation PlannerBed Layout Planner

After slicing

G-code Viewer & Preflight
View all 3D tools
STL toolsSTL ViewerSTL Quality CheckerSTL Print Preflight CheckerSTL Repair ToolSTL Watertight CheckerSTL Manifold CheckerSTL Dimensions CheckerSTL Scale ToolSTL Wall Thickness CheckerSTL Overhang CheckerSTL SplitterSTL Volume CalculatorSTL Triangle CounterSTL File Size ReducerSTL to 3MF Converter
3MF tools3MF Viewer3MF Quality Checker3MF Print Preflight Checker3MF Repair Tool3MF Watertight Checker3MF Manifold Checker3MF Dimensions Checker3MF Wall Thickness Checker3MF Overhang Checker3MF Volume Calculator3MF Triangle Counter3MF to STL Converter
MaterialsGuidesExamplesContact
Home›Compare 3D Printing Materials›PETG vs ASA

PETG vs ASA: Which Filament Should You Use?

PETG usually reduces setup burden; ASA is the more specialised option for weather-exposed parts.

Choose PETG when

  • The part is primarily indoor or lightly exposed.

Choose ASA when

  • UV and weather resistance are central requirements.

Requirements that decide this pair

RequirementPETGASA
Sheltered prototypeA candidate when straightforward functional prototyping is the main task.Enclosure and warp control may add unnecessary prototype preparation.
Sustained sunlightCheck the exact product evidence before extending a prototype into outdoor service.Investigate a UV-resistant formulation with the intended colour and exposure.
Loaded outdoor coverCheck mounting creep and actual surface temperature.Check the same service conditions plus the documented printing environment.

An outdoor cover needs more than a weather-resistance label

A hypothetical 120 x 80 mm outdoor sensor cover has four mounts and a cable opening. PETG may serve a sheltered prototype; ASA is worth evaluating for sustained sunlight using exact product guidance. Check mounting loads, actual surface heat and a separate gasket or drainage strategy. Neither material selection nor a closed mesh establishes water sealing.

Hypothetical application, not an InspectMesh physical material test.

When the initial choice changes

A shaded temporary cover may not justify ASA enclosure preparation. A sun-heated, loaded cover may require a different grade or redesign even if ASA is shortlisted. Validate the chosen colour and formulation under the actual exposure.

Evidence that would change this choice

Conditional choice: Keep PETG when its known process answers the job; shortlist ASA when sunlight exposure provides a reason and preparation can be verified.

The ASA product recommends a skirt or enclosure. That recommendation cannot mark every ASA impossible; a selected product or printer requirement must still be respected. Unknown setup evidence is not a pass.

Next evidence to collect: For the four-mount outdoor cover, record actual part-temperature range, fastening constraint and exposure duration before interpreting an outdoor family band. Check the selected printer, surface and enclosure instructions as a separate preparation decision; retain water paths and gasket testing independently.

Read the evidence needed for a heated part

Family context explains the trade-off above. The named examples below retain their own formulation and test scope.

Published product examples, separate from the family view

These are identified formulations chosen to show how to read evidence. Selecting a family does not select a brand for your part. HDT rows are grouped by reported test load, never by the highest temperature. An absent matching-load result remains unavailable; matching a load alone does not establish matching specimen or conditioning.

Prusament PETG evidence · Prusament ASA evidence

Compare reported properties and conditions, without an overall winner
Property Prusament PETG Prusament ASA Comparison scope
Density

1.27 g/cm³

Prusa Polymers, v1.1
Source conditions

Method: ISO 1183; load: not specified; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-10-29.

1.07 g/cm³

Prusa Polymers, v1.1
Source conditions

Method: ISO 1183; load: not specified; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-10-29.

Separate published values

Different or unspecified specimen, conditioning, test temperature. Read each source separately; these values do not establish which material performs better in your part.

Heat deflection temperature (1.80 MPa)

68 °C

Prusa Polymers, v1.1
Source conditions

Method: ISO 75; load: 1.80 MPa; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-10-29.

86 °C

Prusa Polymers, v1.1
Source conditions

Method: ISO 75; load: 1.80 MPa; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-10-29.

Separate published values

Different or unspecified specimen, orientation, conditioning, test temperature. Read each source separately; these values do not establish which material performs better in your part.

Tensile modulus

1.5 ± 0.1 GPa

Prusa Polymers, v1.1
Source conditions

Method: ISO 527-1; load: not specified; specimen: MK3; Slic3r Prusa Edition 1.40.0; 0.20 mm FAST; 100% rectilinear infill; 2 perimeters; no top/bottom; 250 °C nozzle; 80 °C bed; orientation: Horizontal; conditioning: not specified; test temperature: not specified.

p. 2, printed-specimen table; p. 3, footnote setup. Checked 2026-10-29.

1.6 ± 0.1 GPa

Prusa Polymers, v1.1
Source conditions

Method: ISO 527-1; load: not specified; specimen: MK3S; Slic3r Prusa Edition 2.0.0; 0.20 mm FAST; 100% rectilinear infill; 2 perimeters; no top/bottom; 265 °C nozzle; 110 °C bed; orientation: Horizontal; conditioning: not specified; test temperature: not specified.

p. 2, printed-specimen table; p. 3, setup footnote. Checked 2026-10-29.

Separate published values

Different or unspecified specimen, conditioning, test temperature. Read each source separately; these values do not establish which material performs better in your part.

HDT is a loaded deflection test, not a continuous service limit. Modulus measures stiffness; it is not impact strength. Shore A and D remain different scales.

Open this pair in the comparison tool

Prepare the exact formulation

Use a PETG-specific surface/profile for the prototype. For ASA, verify enclosure, ventilation and warp control; compare cooled mount positions with the mating enclosure.

Use the spool maker's settings and datasheet; a family-wide nozzle range is not a qualified profile.

Sources for this decision

  • Prusa Research: PETG material guidance (checked 2026-10-09)
  • Prusa Research: ASA material guidance (checked 2026-10-09)

Sources describe the material families and printing preparation. Application dimensions and qualification steps above are illustrative design decisions.

PETG guide · ASA guide · Use the selector

Reviewed 2026-11-03.

Get occasional updates on new tools and practical 3D-print guides.

Verification (required)

Enter your email to start verification.

Simple, browser-friendly tools for better 3D prints.

ExamplesPrivacyCookiesContact