InspectMesh
Tools

Planning & calibration

3D Printer Fit Checker3D PrintersCompare 3D Printers3D Print Cost Calculator3D Printing Price CalculatorFilament Length CalculatorFlow Rate CalculatorTolerance & ClearanceShrinkage CalculatorOrientation PlannerBed Layout Planner

After slicing

G-code Viewer & Preflight
View all 3D tools
STL toolsSTL ViewerSTL Quality CheckerSTL Print Preflight CheckerSTL Repair ToolSTL Watertight CheckerSTL Manifold CheckerSTL Dimensions CheckerSTL Scale ToolSTL Wall Thickness CheckerSTL Overhang CheckerSTL SplitterSTL Volume CalculatorSTL Triangle CounterSTL File Size ReducerSTL to 3MF Converter
3MF tools3MF Viewer3MF Quality Checker3MF Print Preflight Checker3MF Repair Tool3MF Watertight Checker3MF Manifold Checker3MF Dimensions Checker3MF Wall Thickness Checker3MF Overhang Checker3MF Volume Calculator3MF Triangle Counter3MF to STL Converter
MaterialsGuidesExamplesContact
Home›Compare 3D Printing Materials›PETG vs PA / Nylon

PETG vs PA / Nylon: Which Filament Should You Use?

PETG is generally easier to prepare; nylon is a tougher engineering family with much higher moisture sensitivity.

Choose PETG when

  • You value accessible general-purpose printing.

Choose PA / Nylon when

  • Wear and toughness justify drying discipline.

Requirements that decide this pair

RequirementPETGPA / Nylon
Accessible fit prototypeA candidate for checking the basic geometry with a familiar process.Drying and conditioning add variables before the fit result is meaningful.
Repeated slidingValidate the exact sliding contact and required duty.A wear-oriented candidate; choose PA chemistry, reinforcement and mating-surface evidence.
Humidity and final dimensionsRecord the service conditions and exact grade.Measure in a defined conditioned state; PA6, PA12 and filled grades are different cases.

A sliding guide requires moisture and wear evidence

For a 50 mm sliding guide, PETG can be a candidate for an accessible fit prototype. A nylon grade becomes worth evaluating when repeated sliding, wear or toughness dominate. Record the mating surface and humidity conditions; measure the guide after printing and after conditioning for service. No wear cycle count is claimed here.

Hypothetical application, not an InspectMesh physical material test.

When the initial choice changes

A low-duty dry indoor guide can favour PETG simplicity. A humid precision fit can rule out an unqualified nylon choice because conditioning changes dimensions. PA6, PA12 and fibre-filled products need separate evidence.

Evidence that would change this choice

Conditional choice: Keep the PETG workflow unless a specified PA grade has relevant wear or dimensional evidence for the changed job.

The nylon example is unfilled PA11, not PA6 or a filled grade. Its mechanical moisture-conditioning state is unspecified; do not compare it as a dry-versus-wet test or infer a scale correction.

Next evidence to collect: For the 50 mm sliding guide, retain cooled reference dimensions separately from service-condition readings at the same axes and mating references. Name the unfilled PA11 grade, preparation and exposure duration. Missing conditioned data remains unknown; a mass percentage cannot become a universal nylon scale correction.

Compare reference and service-condition fit

Family context explains the trade-off above. The named examples below retain their own formulation and test scope.

Published product examples, separate from the family view

These are identified formulations chosen to show how to read evidence. Selecting a family does not select a brand for your part. HDT rows are grouped by reported test load, never by the highest temperature. An absent matching-load result remains unavailable; matching a load alone does not establish matching specimen or conditioning.

Prusament PETG evidence · Prusament PA11 evidence

Compare reported properties and conditions, without an overall winner
Property Prusament PETG Prusament PA11 Comparison scope
Density

1.27 g/cm³

Prusa Polymers, v1.1
Source conditions

Method: ISO 1183; load: not specified; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-10-29.

1.02 g/cm³

Prusa Polymers, v1.0
Source conditions

Method: ISO 1183; load: not specified; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-10-29.

Separate published values

Different or unspecified specimen, conditioning, test temperature. Read each source separately; these values do not establish which material performs better in your part.

Heat deflection temperature (1.80 MPa)

68 °C

Prusa Polymers, v1.1
Source conditions

Method: ISO 75; load: 1.80 MPa; specimen: not specified; orientation: not specified; conditioning: not specified; test temperature: not specified.

p. 2, typical properties. Checked 2026-10-29.

Not found in this example; not zero. Unavailable

A numeric result is not published for one or both selected examples. Missing is not zero.

Tensile modulus

1.5 ± 0.1 GPa

Prusa Polymers, v1.1
Source conditions

Method: ISO 527-1; load: not specified; specimen: MK3; Slic3r Prusa Edition 1.40.0; 0.20 mm FAST; 100% rectilinear infill; 2 perimeters; no top/bottom; 250 °C nozzle; 80 °C bed; orientation: Horizontal; conditioning: not specified; test temperature: not specified.

p. 2, printed-specimen table; p. 3, footnote setup. Checked 2026-10-29.

1.2 ± 0 GPa

Prusa Polymers, v1.0
Source conditions

Method: ISO 527-1; load: not specified; specimen: CORE One+ firmware 6.4.0; 0.4 mm High-Flow CHT; PrusaSlicer 2.9.6; 0.20 mm layers; 100% rectilinear; 2 perimeters; no top/bottom; 275 °C nozzle; 100 °C bed; 55 °C chamber; orientation: Horizontal; conditioning: not specified; test temperature: not specified.

p. 2, printed-specimen table; p. 3, footnote setup. Checked 2026-10-29.

Separate published values

Different or unspecified specimen, conditioning, test temperature. Read each source separately; these values do not establish which material performs better in your part.

HDT is a loaded deflection test, not a continuous service limit. Modulus measures stiffness; it is not impact strength. Shore A and D remain different scales.

Open this pair in the comparison tool

Prepare the exact formulation

Follow exact nylon drying and storage instructions and confirm the bed/nozzle arrangement. Reinforced nylon can need abrasion-resistant hardware; do not transfer an unfilled spool profile automatically.

Use the spool maker's settings and datasheet; a family-wide nozzle range is not a qualified profile.

Sources for this decision

  • Prusa Research: PETG material guidance (checked 2026-10-09)
  • Prusa Research: PA-NYLON material guidance (checked 2026-10-09)

Sources describe the material families and printing preparation. Application dimensions and qualification steps above are illustrative design decisions.

PETG guide · PA / Nylon guide · Use the selector

Reviewed 2026-11-03.

Get occasional updates on new tools and practical 3D-print guides.

Verification (required)

Enter your email to start verification.

Simple, browser-friendly tools for better 3D prints.

ExamplesPrivacyCookiesContact